Machinable Ceramic Materials - MACOR® (Corning Glass)

PROPERTY UNITS VALUE
 Mechanical    
 Density gm/cc 2.52
 Hardness Knoop 250
 Tensile Strength kpsi -
 Modulus of Elasticity psi x 106 9.3
 Flexural Strength kpsi 15
 Compressive  Strength kpsi 50
 Poisson's Ratio - -
 Fracture Toughness MPa m1/2 -
 Electrical    
 Dielectric Strength ac volts/mil 1000
 Dielectric Constant (at 1 MHz) -
 Volume Resistivity ohm-cm2/cm >1014
 Thermal    
 Coefficient of
 Thermal Expansion
x10-6/°C 9.4
 Thermal Conductivity W/m°K 1.7
 Specific Heat cal/g°C -
 Max Working Temp °C 1000
 Shock Resistance °C -
All properties are at room temperature unless otherwise noted.

Engineering data are representative, and are not intended as absolute nor warrantable. Manufacturer’s Data shown is blended from multiple sources and therefore illustrates the marketplace.

This technical information has been contributed by
Insaco Incorporated

Click here to find suppliers


Home |  About Us |  Back To Technical Library |  Contact Us
Copyright © 1996-2010 JobShop.com. All Rights Reserved.
General or Technical Questions? E-mail support@JobShop.com